Quick Details

  • Condition: New
  • Storage: Strong acid Sulfuric Acid
  • Drive Wheel: 6x4
  • Horsepower: 351 - 450hp
  • Transmission Type: Manual
  • Fuel Type: Diesel
  • Tank Volume: 15001 - 30000L
  • Engine Capacity: 9.726L
  • Dimensions (L x W x H) (mm): 10000x2496x3548
  • Brand Name: TIC
  • Place of Origin: Hubei, China
  • Model Number: TIC9402GFW
  • Gross Vehicle Weight: 41000
  • Color: White

Packaging & Delivery

Packaging Details By containers
truck by Ro-Ro or Bulk base on the ship and port in your country. If the truck on the deck,
we will spray antirust paint with free. Usually we will put the truck in cabin of the ship.
Port Shanghai

10sets sales 3 axles sulfuric acid tanker semi trailer, for Afica Zambia market

 

Acid tank  body Customization, Cost Control Built How You Want it, at a Price You Can Afford. for sale

 

call:+86-152 -7135-7675 We make the Acid tank Truck Parts

 

we can make with the capacity as your request. Good design for long using life.

 

Specification  18000---19,000 liter

  tanker trailer

Sulfuric acid tank trailer 

Sulfuric acid tanker trailer  with F2000 Shacman tractor 

Sulfuric acid tanker trailer  with F2000 Shacman tractor delivery to port Photod

Sulfuric acid tanker trailer  with F2000 Shacman tractor shipped by RORO car carrier ship.

specifications just for reference

DIMENSIONS

Tare  Weight

8500kg

Payload

31500 kg

Total  Weight

40000kg

Overall  Length

Refer drawing 10000mm

Overall  Width

Refer drawing mm (maximum 2500mm)

Overall  Height

Refer drawing  3500mm

Wheel track

Refer drawing mm

Wheel base

Refer drawing mm

STANDARD SPECIFICATION

Main  Frame

Heavy duty and extra durability designed; Opting for high tensile steel Q345B,welded by automatic Submerged-Arc processes 505mm Height, Top Flange 14mm,width 140mm; Middle Flange 6mm ;Bottom Flange 16mm,width 140mm  

 

Axle

Three Units of BPW axles.  

Suspension

3-axle spring Suspension   

Landing Gear

Two-speed ,manual operation, heavy duty landing gear

Wheel Rim

Twelve units of 8.25or9.0wide x 10 stud (tubeless rim)

Tyre

Twelve units of 12R-22.5 tyres (tubeless)  

Spare Wheel Carrier

two sets of spare wheel carrier including a riser  

Pneumatic Braking System

30/30 spring brake chamber (S Cam); eliable local brand 40L air tank ;  reliable local brand standard coppery air-connector. With ABS

Electrical  System

24V 7-pin socket; reliable local brand standard red rear lights, orange turning lights, red rear reflectors, 3 orange side lights and 3 orange side reflectors each side 6, standard Cable.   

Tank

19,000 litres capacity  

 

Shell baffles 6 mm  carbon steel

 

Walkway and top tank; ladder end or side of tank

Tank fittings

Manhole covers top filler and with spillbox,

 Bottom coupling DN80 discharge system 

Painting

Sand blasting before painting; two coats of primer, anti corrosion, two coats of finish painting; (black chassis, blue tank or as client requirement)

Accessory

One trailer tool box , One 200L water tank.

 

 

Acid  tank  body steel lined PE plastic lining manhole and covers ,optional full Plastic covers!

 

 

Service/Fluid : HCl acid 32%/ Caustic Soda NaOH 32%/ Sodium

Volume : 16000 

Dimension :

- Length : 5200 -6000 mm

- Width : 2000 -2500 mm

- Height : 1400 - 2300 mm

Material :steel cover + lining PE

Type : Ref. to attached drawing

Structure : with two seperated chambers

Other : (Manhole, Discharge Valve, Pressure Relief Vent, ...) type,

Hypochlorite NaClO 12%/ Ferrous chloride 40%

spec., quantity ... follow Manuf. Design, suitable for storing

and transporting of chemicals.

  Factory LDPE plastic lining Roll forming machine and dishhead forming machine

 

 Acid tank Truck upper tank body steel lined PE /plastic lining shipping by containers

Acid tank Truck upper tank body steel lined PE /plastic lining shipping by Bulk ship .

Acid tank Truck upper tank body steel lined PE /plastic lining shipping by truck chassis to  China border

Customize  Truck

Cell:  0086 152 7 135 7635   ; 0086 152 7 135 7675 
WhatsApp: 8615271357675    tictrucks#gmail.com    

 

The corrosion resistance of polyethylene (PE)

 

 Chemical Resistance Chart for LDPE (Low Density Polyethylene)
The chemical resistance chart below is a general guide only. Please contact us for specific applications

 

LDPE & HDPE  polyethylene  resistance listed by chemical
1.4-dioxane LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days of constant exposure.
Acetaldehyde LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure. LDPE - immediate damage may occur.
Acetic Acid 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Acetic Acid, glacial 50% LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50 C° -
immediate damage may occur.
Acetone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Allyl Alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Aluminum salts LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amino acids LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonia LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium carbonate,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium phosphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amyl chloride HDPE at 20C° shows some effect after 7 days of constant exposure. HDPE at 50C° and LDPE at 20C°-50C° -
immediate damage may occur. Not recommended for continuous use.
Aniline LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure.
Benzene LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Benzyl alcohol LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Boric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Bromine LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Butyric acid LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Calcium chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium hydroxide
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium sulphate No data is available at this time.
Carbon tetrachloride HDPE at 20C° shows little or no damage after 30 days. LDPE at 20C° and HDPE at 50C° show some effect
after 7 days of constant exposure. LDPE at 50C° not recommended.
Chlorobenzene Immediate damage may occur. Not recommended for continuous use.
Chloroform HDPE and LDPE at 20C° show some effect after 7 days. At -50C° - immediate damage may occur. Not
recommended for continuous use.
Chlorine 10% in water HDPE and LDPE at 20C° shows little or no damage after 30 days. LDPE at 50C° shows damage and is not
recommended.
Chromic acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Chromic acid 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Citric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Cresol HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Cyclohexane LDPE and HDPE at 50C° - immediate damage may occur. HDPE and LDPE at 20C° show some effect after 7
days of constant exposure.
Diethyl ketone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Dimethylsulfoxide LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethanol 95% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. Ethyl acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethyl benzene HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Ethylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethylene oxide HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° and LDPE/ HDPE
at 50C° show some effect after 7 days.
Ferric chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluoride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluorine HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° shows some effect
after 7 days. Neither HDPE or LDPE are recommended at 50C°.
Formaldehyde 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Formaldehyde 40% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Glycerol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Heating oil No further data is available at this time.
Hexane HDPE at 20C° shows little or no damage after 30 days continuous use and at 50 C° shows some effect after 7
days. LDPE not recommended at any temperature.
Hydrochloric acid 5% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 35% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrocyanic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 4% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 48% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 3% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 30% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isobutyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isopropyl acetate No data is available at this time.
Isopropyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Kerosene LDPE and HDPE at 20C° show some effect after 7 days. HDPE and LDPE not recommended at 50C°, as
immediate damage may occur.
Lactic Acid 10 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lactic Acid 90 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lead acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Metallic salts, dissolved No data is available at this time.
Methanoic acid 100% No data is available at this time.
Methanol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Methyl ethyl ketone Immediate damage may occur. Not recommended for continuous use.
Methyl propyl ketone HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Methylene chloride HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Mineral oil LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° may
show immediate damage and is not recommended.
n-amyl acetate LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days or constant exposure.
n-butyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
n-octane LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Nitric acid 50 % LDPE at 20C° shows little or damage after 30 days. HDPE at 20C° and LDPE at 50C° show effect after 7 days.
HDPE at 50C° shows immediate damage and is not recommended.
Nitric acid 70 % HDPE and LDPE at 20C° show some effect after 7 days. Both at 50C° show immediate damage and are not
recommended.
Oleic acid HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C°-50C° shows
immediate damage and is not recommended.
Oxalic acid LDPE at 20C° shows some effect after 7 days. HDPE at 20C° and both HDPE and LDPE at 50C° show little or
no damage after 30 days.
Ozone HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at
50C° show immediate damage and are not recommended.
Perchloric acid HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 50C° show immediate damage and are not recommended.
Perchloric ethylene HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phenol HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phosphoric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Phosphoric acid 85% HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
immediate damage and is not recommended.
Phosphorous trichloride HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° has no
data available. HDPE at 50C° shows some effect after 7 days.
Potassium acetate No data is available at this time.
Potassium bromide No data is available at this time.
Potassium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide
concentrated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium permanganate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Propylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Pyridine Immediate damage may occur. Not recommended for continuous use.
Salicylic acid, saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium chloride,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium dichromate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hydroxide 1% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C°-50C° shows
some effect after 7 days.
Sodium hydroxide 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hypochlorite 15% HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C° is suitable but
at 50C° shows some effect after 7 days.
Sodium nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sucrose LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulphide No additional information is available at this time.
Sulfuric acid 6% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 60% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 98% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C° shoes effect
after 7 days and is not recommended for use at 50C°.
Tannic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Tetrahydrofuran HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Toluene LDPE at 20C° show some effect after 7 day of constant exposure. HDPE at 20C°-50C° and LDPE at 50C°
show immediate damage and are not recommended.
Trichloracetic acid HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Trichlorethane Immediate damage may occur. Not recommended for continuous use.
Turpentine oil HDPE and LDPE at 20C° show some effect after 7 day of constant exposure. HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Urea LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Xylene HDPE at 20C° shows some effect after 7 day of constant exposure. LDPE at 20-50C° and HDPE at 50C° show
immediate damage and are not recommended.
Zinc chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.

China
The supplier supports Trade Assurance – A free service that protects your orders from payment to delivery.
Supplier's Trade Assurance Limit:
Learn More

WhatsApp: 8615271357675