Quick Details

  • Use: Truck Trailer
  • Type: Semi-Trailer
  • Material: Steel
  • Certification: CCC BV SGS
  • Size: 11400*2500*3450mm
  • OEM No.: DRZ9400GHY
  • Max Payload: 33T-60T
  • Place of Origin: Hubei, China
  • Brand Name: DRZE
  • Color: White
  • Keywords: Acid tanker semitrailer
  • Tanker Body Material: Carbon Steel Q235B, 6 mm
  • Axle: 3 FUWU / L1 /BPW 13 ton
  • Tire: 12R22.5 tubeless tire with two spare tire, 14 pieces
  • Wheel rim: 9.0-22.5 wheel rim, 14 pieces
  • Tank Body: V shape
  • MOB: +86-152-71357675

Packaging & Delivery

Packaging Details Parts SKD By containers WhatsApp:86.152.7135.7675 Skype:tomsongking
Trucks /Trailers by Ro-Ro or Bulk base on the ship and port in your country. If the truck on the deck,
we will spray antirust paint with free. Usually we will put the truck in cabin of the ship.
Port Shanghai

Sulphuric Acid Tanker Trailer V shape 22000L for Zambia

 

3 axles sulfuric acid tanker semi trailer, for Afica Zambia market

 

 


Acid tanker material can be high quality carbon steel,stainless steel SS316L.
this V shape acid tanker trailer is equipped with 3 units 13T BPW axles or FUWA axles.
with heavy duty spring suspension or airbag suspension. -

Main Dimensions
Overall Length11400mm
Overall Height3400mm
Overall Width2500 mm
Tare Weight8800-9200 KGS
Loading Capacity38000 kgs
Tank Body
ShapeV shape
Total Volume(m3)21-22 CBM
Tanker Body MaterialCarbon Steel Q235B, 6 mm
End plateCarbon Steel Q235B, 6 mm
Chassis
Axle3 axles
L1 / FUWA / BPW 13 ton
Landing GearJOST brand Two-speed, manual operating, heavy duty landing gear
King PinJOST brand 2” bolt-in king pin
SuspensionHeavy duty type mechanical suspension
Pneumatic Braking SystemWABCO RE 4 relay valve; T30/30+T30 Spring brake chamber; 40L air tanks.
Wheel rim9.0-22.5 wheel rim, 14 pieces
Tire12R22.5 tubeless tire with two spare tire, 14 pieces
Spare wheel carrier2 per tank
MudguardsCarbon steel with flaps
Water tankTop lid with chain with bottom valve
PaintingComplete Chassis sand blasting to clean rust, 1 coat of anticorrosive prime, 2 coats of final paint
TaillightsAnti theft Top LED wonder lights 2 indicator and 2 brake
Anti theft Bottom LED wonder lights 4 indicator, 4 brake, 1
reverse and 2 number plate
AccessoriesOne standard tool box

  Factory LDPE plastic lining Roll forming machine and dishhead forming machine

 

 Acid tank Truck upper tank body steel lined PE /plastic lining shipping by containers

 

Acid tank Truck upper tank body steel lined PE /plastic lining shipping by Bulk ship .

 

Acid tank Truck upper tank body steel lined PE /plastic lining shipping by truck chassis to  China border

Customize  Truck

Cell:  0086 152 7 135 7635   ; 0086 152 7 135 7675 
WhatsApp: 8615271357675    tictrucks#gmail.com    
 

 

The corrosion resistance of polyethylene (PE)

 

 Chemical Resistance Chart for LDPE (Low Density Polyethylene)
The chemical resistance chart below is a general guide only. Please contact us for specific applications

  

 

LDPE & HDPE  polyethylene  resistance listed by chemical
1.4-dioxane LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days of constant exposure.
Acetaldehyde LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure. LDPE - immediate damage may occur.
Acetic Acid 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Acetic Acid, glacial 50% LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50 C° -
immediate damage may occur.
Acetone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Allyl Alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Aluminum salts LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amino acids LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonia LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium carbonate,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium phosphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ammonium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Amyl chloride HDPE at 20C° shows some effect after 7 days of constant exposure. HDPE at 50C° and LDPE at 20C°-50C° -
immediate damage may occur. Not recommended for continuous use.
Aniline LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE at 50C° shows
some effect after 7 days of constant exposure.
Benzene LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Benzyl alcohol LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Boric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Bromine LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Butyric acid LDPE and HDPE at 50C° - immediate damage may occur. HDPE at 20C° shows some effect after 7 days of
constant exposure.
Calcium chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium hydroxide
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Calcium sulphate No data is available at this time.
Carbon tetrachloride HDPE at 20C° shows little or no damage after 30 days. LDPE at 20C° and HDPE at 50C° show some effect
after 7 days of constant exposure. LDPE at 50C° not recommended.
Chlorobenzene Immediate damage may occur. Not recommended for continuous use.
Chloroform HDPE and LDPE at 20C° show some effect after 7 days. At -50C° - immediate damage may occur. Not
recommended for continuous use.
Chlorine 10% in water HDPE and LDPE at 20C° shows little or no damage after 30 days. LDPE at 50C° shows damage and is not
recommended.
Chromic acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Chromic acid 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Citric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Cresol HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Cyclohexane LDPE and HDPE at 50C° - immediate damage may occur. HDPE and LDPE at 20C° show some effect after 7
days of constant exposure.
Diethyl ketone LDPE and HDPE at 20C°-50C° - damage may occur. Not recommended for continuous use.
Dimethylsulfoxide LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethanol 95% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. Ethyl acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethyl benzene HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° show immediate
damage and are not recommended for continuous use.
Ethylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Ethylene oxide HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° and LDPE/ HDPE
at 50C° show some effect after 7 days.
Ferric chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluoride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Fluorine HDPE at 20C° shows little or no damage after 30 days of constant exposure. LDPE at 20C° shows some effect
after 7 days. Neither HDPE or LDPE are recommended at 50C°.
Formaldehyde 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Formaldehyde 40% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Glycerol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Heating oil No further data is available at this time.
Hexane HDPE at 20C° shows little or no damage after 30 days continuous use and at 50 C° shows some effect after 7
days. LDPE not recommended at any temperature.
Hydrochloric acid 5% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrochloric acid 35% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrocyanic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 4% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrofluoric acid 48% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 3% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Hydrogen peroxide 30% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isobutyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Isopropyl acetate No data is available at this time.
Isopropyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Kerosene LDPE and HDPE at 20C° show some effect after 7 days. HDPE and LDPE not recommended at 50C°, as
immediate damage may occur.
Lactic Acid 10 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lactic Acid 90 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Lead acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Metallic salts, dissolved No data is available at this time.
Methanoic acid 100% No data is available at this time.
Methanol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Methyl ethyl ketone Immediate damage may occur. Not recommended for continuous use.
Methyl propyl ketone HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Methylene chloride HDPE at 20C° shows some effect after 7 days. LDPE at 20C°-50C° and HDPE at 50C° - Immediate damage
may occur. Not recommended for continuous use.
Mineral oil LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° may
show immediate damage and is not recommended.
n-amyl acetate LDPE and HDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
some effect after 7 days or constant exposure.
n-butyl alcohol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
n-octane LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Nitric acid 50 % LDPE at 20C° shows little or damage after 30 days. HDPE at 20C° and LDPE at 50C° show effect after 7 days.
HDPE at 50C° shows immediate damage and is not recommended.
Nitric acid 70 % HDPE and LDPE at 20C° show some effect after 7 days. Both at 50C° show immediate damage and are not
recommended.
Oleic acid HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C°-50C° shows
immediate damage and is not recommended.
Oxalic acid LDPE at 20C° shows some effect after 7 days. HDPE at 20C° and both HDPE and LDPE at 50C° show little or
no damage after 30 days.
Ozone HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at
50C° show immediate damage and are not recommended.
Perchloric acid HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. HDPE and LDPE at 50C° show immediate damage and are not recommended.
Perchloric ethylene HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phenol HDPE and LDPE at 20C°-50C° show immediate damage and are not recommended.
Phosphoric acid 10% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Phosphoric acid 85% HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° shows
immediate damage and is not recommended.
Phosphorous trichloride HDPE and LDPE at 20C° show little or no damage after 30 days of constant exposure. LDPE at 50C° has no
data available. HDPE at 50C° shows some effect after 7 days.
Potassium acetate No data is available at this time.
Potassium bromide No data is available at this time.
Potassium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide 5 % LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium hydroxide
concentrated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Potassium permanganate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Propylene glycol LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Pyridine Immediate damage may occur. Not recommended for continuous use.
Salicylic acid, saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver acetate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Silver nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium carbonate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium chloride,
saturated LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium dichromate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hydroxide 1% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C°-50C° shows
some effect after 7 days.
Sodium hydroxide 50% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium hypochlorite 15% HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure. LDPE at 20C° is suitable but
at 50C° shows some effect after 7 days.
Sodium nitrate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sodium sulphate LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sucrose LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulphide No additional information is available at this time.
Sulfuric acid 6% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 20% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 60% LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Sulfuric acid 98% LDPE at 20C°-50C° shows little or no damage after 30 days of constant exposure. HDPE at 20C° shoes effect
after 7 days and is not recommended for use at 50C°.
Tannic acid LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Tetrahydrofuran HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Toluene LDPE at 20C° show some effect after 7 day of constant exposure. HDPE at 20C°-50C° and LDPE at 50C°
show immediate damage and are not recommended.
Trichloracetic acid HDPE and LDPE at 20C° show some effect after 7 day of constant exposure.HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Trichlorethane Immediate damage may occur. Not recommended for continuous use.
Turpentine oil HDPE and LDPE at 20C° show some effect after 7 day of constant exposure. HDPE and LDPE at 50C° show
immediate damage and are not recommended.
Urea LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.
Xylene HDPE at 20C° shows some effect after 7 day of constant exposure. LDPE at 20-50C° and HDPE at 50C° show
immediate damage and are not recommended.
Zinc chloride LDPE and HDPE at 20C°-50C° show little or no damage after 30 days of constant exposure.

China
The supplier supports Trade Assurance – A free service that protects your orders from payment to delivery.